文档简介
常用英语词汇
Sharlin
20150925前模/定模/母模cavity(cavity也叫模穴)后模/动模/公模core(core统称模芯,模仁)枕位、穿插、碰穿shutoff直径diameter圆角/半径radius重叠overlap导向槽guidingslot(不动的部分)倒扣undercut切线tangent脱模角度、拔模锥度draftangle分模线/分型面partingline=PL行位分型线sliderPL模具用语行位、滑块slider(移动的部分)行位孔sliderhole行位/滑块运动方向slidermovementdirection(箭头所示)行位夹线sliderline(红色线条)热流道hotrunner便于出模releasethetooleasily后模镶件coreinsert排气镶件gasventinsert镶针insertpin为了更好的走胶toimproveplasticflowing/forbettermaterialflowing模穴号刻在顶针上engravethecavity#ontheE/Ps产品刻字位置letteringlocation刻字字宽width1.2mm,字凸convex0.07mm绝缘resistcoating相切半径tangentradius电镀夹片rackingtab斜顶lifter内圈分型线insidepartinglinedemold脱模aspertheissuesabove上述问题扣位clipintersect[,intə'sekt]vi.相交,交叉(两条直线或两个平面相交)vt.横断,横切;贯穿正段差是后模比前模小,逆段差就是前模比后模小。都用step色粉colorant水口残留GatevestigeEPEfoam珍珠棉(ExpandAplePolyEphylene)损耗率scrapratescrap:废弃,残留标准样板mastersample限度样板boundarysample颜色限度样品colorboundarysample缺陷样板defectsample产品V/P切换压力为57.5MPaPressureatV/Pswitchoveris57.5Mpa模流分析moldflowanalysis体积收缩volumetricshrinkageatejection缩痕估算sinkmarksestimate总体变形alleffectsdeflectionX.Y方向变形deflection,alleffects:X.Ycomponent蚀纹texture,graining贴胶带felttape吸塑包装blisterpackaging潜进胶SubgateTunnel-gate,搭底进胶Overlapgate/tabgate点进胶/点胶口pinpointgate翻译实例1由于加工精度问题,行位孔与模仁上骨位深度很难刚好做平,现将产品骨位此处减胶0.05mm,请知悉,左右两个孔一样.Becauseoftheaccuracyofthemanufacture,itisdifficulttomakethesliderholethesamelevelwiththecoredepth,sowesuggestreducing0.05mmplasticontheribs,pleasemakethesamechangetobothLH&RHholes.3怕结合力不好,建议第一色做孔,增加结合力.Wesuggestaddsomeholesonthefirstshotinordertoincreasetheadhesionstrength4为利于模具制作及简化分型面,建议箭头所指侧面减胶拔模到后模.Wesuggestthebyarrowindicatedsidereducematerialandmakingintothecoreinordertomanufacturethetooleasierandsimplifythepartingline.5建议上图中两个绿色孔侧面沿行位运动方向做脱模斜度Wesuggestaddingdrafton2greensidesalongthemovingdirectionofslider.6为了保证外观面,建议将PL面下移0.2MM。SuggestloweringthePL0.2MMtoavoidthePLonthevisiblesurface.7此绿色面没有出模角,建议以减胶方式做3度的出模角以便行位出模。Nodraftingreenarea,suggestreducingplasticanddraftangle3degreetoreleasetheslidereasily.8此处掏胶掏进去0.6MM.Herereduce0.6mmplasticinjection.9此处打1圆点或2圆点作为型腔号,请确认!Make1dotor2sasthecavitynumber10产品此两处侧面绿色面为直身面,为防止产品此面脱花或拉伤,需增加出模角度0.5°(产品减胶)Thegreenareahavenodraftangle,toavoidanyscratch,wewouldliketoreduceplasticfor0.5°draftangle.“R”:RadllGuage(R规)“L”ruler(直尺)“F”Feeler(塞尺)“GONO-GO”:GeneralGuage(通止规)
Fixture(辅具/夹具)
Gage(检具)“T”Taperedclearance(锥形间隙尺)“S”StepGauge(段差尺)试验测试工具fixture/jig(基度)(实验室称呼治具为基度)“V”:VernierCaliper(卡尺)“H”:HeightGuage(高度规)“M”:Micrometer(千分尺)“D”:DialGuage(百分表)“P”:Projector(投影仪)“E”:Visual(目视)“C”:CoordinateMeasureMachine(三次元)“G”:PinGuages(针规)plugguage(塞规)(用于测孔距)Flushgauge(齐平规)黑点 BlackDot披锋 Flash流纹 Flowmark气纹
Gasmark/Flowmark缩水 Sinkmark/shrinkage变形 Deformation亮印 Brightspot擦花/划伤
Scratch碰伤bumpping胶泡 Bubble夹线 Weldline/nitline针孔 pinhole缺胶
ShortShot顶针印
Ejectormark烧焦
Burn打砂印
sandpapermark多胶
extramaterial漏光 LightLeaks模伤/模痕
mouldmark沙粒
Grain/particle亮点 Shiningdot光剂 Bright
liquid/Brightnesschemistry模伤/模痕mouldmark压伤 impression胶件常见缺陷PlatingSequences
电镀步骤Pretreatment前处理Basematerial基材Etching蚀刻Activation活化Accelaration解胶ElectrolessNickel化学镍PlatingSequences电镀步骤Electro-Plating电镀
WattsNickel瓦特镍orPreCopperSemiBrightNickel半光镍BrightNickel光镍AcidCopper酸铜MicroporousNickel微孔镍Chromium铬SatinNickel珍珠镍MicrocrackNickel微裂纹镍2012/11/2223产品设计ProductDesign模具设计MoldDesign模具制造Moul
温馨提示
- 1. 本站所有资源如无特殊说明,都需要本地电脑安装OFFICE2007和PDF阅读器。图纸软件为CAD,CAXA,PROE,UG,SolidWorks等.压缩文件请下载最新的WinRAR软件解压。
- 2. 本站的文档不包含任何第三方提供的附件图纸等,如果需要附件,请联系上传者。文件的所有权益归上传用户所有。
- 3. 本站RAR压缩包中若带图纸,网页内容里面会有图纸预览,若没有图纸预览就没有图纸。
- 4. 未经权益所有人同意不得将文件中的内容挪作商业或盈利用途。
- 5. 人人文库网仅提供信息存储空间,仅对用户上传内容的表现方式做保护处理,对用户上传分享的文档内容本身不做任何修改或编辑,并不能对任何下载内容负责。
- 6. 下载文件中如有侵权或不适当内容,请与我们联系,我们立即纠正。
- 7. 本站不保证下载资源的准确性、安全性和完整性, 同时也不承担用户因使用这些下载资源对自己和他人造成任何形式的伤害或损失。
评论
0/150
提交评论